News

Sheet metal deep drawing: typical defects and how to prevent them at the design stage

Wrinkles, thinning and cracks in deep drawing are prevented at the design stage: radii, blank holder, number of draws and lubrication. Here are the key points.

What deep drawing is

Deep drawing turns a flat sheet into a hollow part, such as covers, trays and housings, by making it flow into the die under the action of the punch.

The most common defects

  • Wrinkles on the flange
  • Excessive wall thinning
  • Cracks at the bottom or on the radii
  • Marks on visible surfaces

How they are prevented

With suitable radii, controlled blank holder force, the right number of draws and lubrication. For deep-drawn parts we split the deformation over several stations.

FAQs

How many draws are needed for a deep-drawn part?

It depends on the ratio between initial and final diameter: deep-drawn parts need several stations, often in a transfer die.

Can stainless steel and aluminium be deep-drawn?

Yes, with specific parameters and radii for each material.

Do you make dies for visible deep-drawn parts?

Yes, for example for furniture, where surface quality is essential.

Let’s talk about your project

Send us your drawing: technical response within 24 working hours.

Send us your drawing. Technical reply within 24 hours.

Talk directly to the people who design and build your die: no middlemen, reliable lead times and certified quality since 1969.

  • Since 1969
  • ISO 9001 · TÜV SÜD
  • Reply in 24 h
  • Sheet 0.05–12 mm